PEMBUATAN La0,8Ca0,2MnO3 SEBAGAI KATODA PADA SOLID OXIDE FUEL CELL (SOFC) DAN KARAKTERISASINYA

Authors

  • Riska Ekawita Departemen Fisika, Fakultas Matematika dan Ilmu Pengetahuan Alam, Universitas Bengkulu

DOI:

https://doi.org/10.19028/jtep.021.2.%25p

Keywords:

solid oxide fuel cell, time of firing, density and porosity, electric conductivity

Abstract

ABSTRACT

 

The making of La0,8Ca0,2MnO3  cathode material of solid oxide fuel cell from lanthanum oxide (La2O3), calcium oxide (CaO), and manganese carbonate hydrate (MnCO3.H2O) has been done using tape casting method. Time of firing the La0,8Ca0,2MnO3  varied. The values of t = 30 minutes, 60 minutes and 120 minutes. Microstructure of these materials was analyzed and characterized by means of their electric conductivity, XRD (x ray diffraction) and SEM (scanning electron microscope). It is found that formulated micro structure is orthorhombic. The result of measurement shows that density is in linear (positive) correlation with increasing of holding time of firing, porosity and coefficient of thermal expansion is negatively correlated with density and electric conductivity is in linear (positive) correlation with increase density.

 

Diterima: 26 Pebruari 2007, Disetujui: 13 Mei 2007

Downloads

Download data is not yet available.

Downloads

Published

2015-10-26

How to Cite

Ekawita, R. (2015). PEMBUATAN La0,8Ca0,2MnO3 SEBAGAI KATODA PADA SOLID OXIDE FUEL CELL (SOFC) DAN KARAKTERISASINYA. Jurnal Keteknikan Pertanian, 21(2). https://doi.org/10.19028/jtep.021.2.%p